CoCr(Ni)W Spherical High-Entropy Alloy (HEA) Powder comprises cobalt, chromium, (nickel), and tungsten. The ratios of the elements and particle sizes can be customized to fit specific requirements.
Warning: Last items in stock!
Availability date:
Shape | Spherical |
Particle Size | -45+5μm, -45+11μm, -75+45μm, -106+37μm, or customized |
Molecular Formula | CoCr(Ni)W |
CoCr(Ni)W Spherical High-Entropy Alloy (HEA) Powder has similar coating properties to tungsten-cobalt-chromium alloys. It has excellent corrosion resistance, resistance to micro-motion and solid particle erosion, which is stable at thermally corrosive elevated temperatures or in oxidizing environments.
Chemical Composition | Particle Size | Note |
Co23.4Cr10Ni7W3.5Ta0.6C | -45+5μm | The ratios and particle sizes can be customized according to specific requirements. |
Co25.5Cr10.5Ni7.5W0.5C | -106+37μm | |
-75+45μm | ||
-45+5μm | ||
Co28.5Cr4.5W1.6Si1C | -45+11μm |
CoCr(Ni)W Spherical High-Entropy Alloy (HEA) Powder should be stored in a sealed container in a dry and cool place, and should not be exposed to air for an extended period of time. We offer vacuum-sealed packaging including 100g/bag, 500g/bag, 1kg/bag, and 25kg/drum, or we can offer customized packaging as per specific requirements.
Heeger Materials respects your privacy, and we will NOT sell or provide your personal data to other third parties, or allow them to use your personal data for their own purposes. However, we would like to send you information from time to time by mail or email about our products and special offers in addition to the interest categories you've selected above. Read our Privacy Policy