CMSX-4 Spherical Nickel Alloy Powder is a single-crystal nickel-based superalloy powder. It has better creep and fatigue resistance at high temperatures widely used in aerospace and industrial fields. Heeger Materials is a professional supplier and manufacturer of high-quality CMSX-4 Spherical Nickel Alloy Powder, offering competitive prices and customized solutions to meet specific requirements.
| Particle Size | 0-25um|15-53um|45-105um|50-150um |
| Materials | NiCoCrWAlTaRe |
CMSX-4 Spherical Nickel Alloy Powder is a high-performance nickel-based alloy powder belonging to a single-crystal alloy, which means it has better creep and fatigue resistance at high temperatures. There is great potential in developing additive manufacturing, laser powder bed fusion (LPBF), or direct energy deposition (DED). HM can supply low-price CMSX-4 Spherical Nickel Alloy Powder with different specifications for various applications in extreme conditions.

CMSX-4 Single Crystal Nickel Based Superalloy Spherical Powder belongs to the nickel based alloy powder range and is selected for controlled particle size distribution, high sphericity, flowability and chemistry suitable for powder processing. It is commonly used in thermal spray coatings, high-temperature additive manufacturing, corrosion-resistant parts, turbine alloy research and brazing-related development. When requesting a quote, confirm nominal composition, particle size cut, oxygen level, morphology, flowability, apparent density, heat or lot documentation and quantity.
For material comparison or adjacent product forms, browse spherical powder, powder materials and thermal spray powder.
What is needed to quote nickel based alloy powder? Share the alloy grade or composition, particle size range, oxygen level, morphology, flowability target, documentation needs and application such as AM, coating or high-temperature service.
Chemical Composition (wt%) | ||||
Ni | Cr | Mo | Re | W |
Bal. | 6.4-6.6 | 0.5-0.7 | 2.8-3.1 | 6.2-6.6 |
Co | Al | Hf | Ta | Ti |
9.3-10.0 | 5.45-5.75 | 0.07-0.12 | 6.3-6.7 | 0.9-1.1 |
Particle Size (μm) | ||||
0-25,15-53,45-105,50-150, or customized | ||||
CMSX-4 Spherical Nickel Alloy Powder should be stored in a sealed container in a dry and cool place, and unexposed to air for an extended time. HM offers vacuum-sealed packaging including 100g/bag, 500g/bag, 1kg/bag, and 25kg/drum, or customized packaging as per specific requirements.

Heeger Materials Inc., a professional supplier, and manufacturer of high-quality Spherical Powder including CMSX-4 Spherical Nickel Alloy Powder, leverages extensive expertise in supply and export to offer competitive prices. We provide customized solutions to meet specific requirements, ensuring exceptional quality and customer satisfaction.
Heeger Materials Inc. was established in 2016 in Colorado, USA. We are a specialized supplier of metals, alloys, ceramics, powders, and other materials catering to research, development, and large-scale industrial production in scientific and industrial sectors.
Heeger Materials respects your privacy, and we will NOT sell or provide your personal data to other third parties, or allow them to use your personal data for their own purposes. However, we would like to send you information from time to time by mail or email about our products and special offers in addition to the interest categories you've selected above. Read our Privacy Policy