| Shape | Spherical / Ball Powder |
| Particle Size | 15-45μm, 15-53μm, 45-75μm, 45-105μm, 75-150μm, customized |
Spherical Superalloy Powder Series belongs to the Spherical Powder range and is selected for controlled material quality, application-specific specifications and reliable supply for research or production use. It is commonly used in custom alloy parts, high-temperature hardware, electrical contacts and application-specific components as well as research, development, specialty manufacturing, laboratory use and industrial material projects. When requesting a quote, confirm composition, form, dimensions, tolerance, heat treatment condition and quantity.
For material comparison or adjacent product forms, browse all products, deposition materials, technical ceramics and Spherical Powder.
What alloy information should be confirmed? Please provide composition, form, dimensions, tolerance, heat treatment condition, quantity and working environment.
A superalloy is a kind of metal material based on iron, nickel, and cobalt, which can work at high temperatures above 600℃ and under certain stress for a long time. It has excellent high-temperature strength, good oxidation resistance and thermal corrosion resistance, good fatigue performance, fracture toughness, and other comprehensive properties, and is also known as a "superalloy".

5-25μm, 15-45μm, 15-53μm, 45-75μm, 45-105μm, 75-150μm. (Various granularities can be customized according to customer requirements)
Grade | Chemical Composition | Particle Size Distribution | |
Elements | Inpurities | ||
IN625(GH3625) | Cr: 20.0-23.0 | Ti: ≤0.40 S: ≤0.015 P: ≤0.015 Y: ≤0.005 | 15-45μm |
IN718(GH4169) | Ni: 50.0-55.0 | O: ≤0.01 | 15-45μm |
IN713(K418) | Cr: 11.5-13.5 | C: 0.08-0.16 | 15-45μm |
IN939 | Cr: 22.0-22.8 | C: 0.13-0.17 | 15-45μm |
IN738LC | Cr: 14.0-16.0 | Ta: 1.00-2.00 | 15-45μm |
Spherical Superalloy Powder should be stored in a sealed container in a dry and cool place, and should not be exposed to air for an extended period of time. We offer vacuum-sealed packaging including 100g/bag, 500g/bag, 1kg/bag, and 25kg/drum, or we can offer customized packaging as per specific requirements.

Heeger Materials respects your privacy, and we will NOT sell or provide your personal data to other third parties, or allow them to use your personal data for their own purposes. However, we would like to send you information from time to time by mail or email about our products and special offers in addition to the interest categories you've selected above. Read our Privacy Policy