Hastelloy X Spherical Superalloy...
View larger SP-1791
New product
Hastelloy X Spherical Superalloy Powder is a nickel-based superalloy that contains substantial amounts of nickel, chromium, iron, and molybdenum, as well as smaller quantities of other elements including cobalt, tungsten, and aluminum. Heeger Materials provides top-quality Spherical Hastelloy X Powder at competitive prices. Customized particle sizes are available based on specific requirements.
Inquiry
Please contact us if you need customized services. We will contact you with the price and availability in 24 hours.
| Particle Size | 15-45μm, 15-53μm, 45-106μm, 75-150μm, or customized |
| Materials | Hastelloy X |
Hastelloy X Spherical Superalloy Powder exhibits an outstanding blend of oxidation resistance, fabricability, and high-temperature strength. It is produced using a vacuum atomization process, ensuring a perfect spherical shape, excellent reproducibility, good flowability, and a low level of oxide content. It is an ideal choice as an additive for 3D printing applications.

Hastelloy X Spherical Superalloy Powder belongs to the spherical powder range and is selected for controlled particle size distribution, high sphericity, flowability and chemistry suitable for powder processing. It is commonly used in custom alloy parts, high-temperature hardware, electrical contacts and application-specific components as well as additive manufacturing, thermal spraying, powder metallurgy, laser cladding, research and specialty alloy development. When requesting a quote, confirm composition, form, dimensions, tolerance, heat treatment condition and quantity.
For material comparison or adjacent product forms, browse spherical powder, powder materials and thermal spray powder.
What alloy information should be confirmed? Please provide composition, form, dimensions, tolerance, heat treatment condition, quantity and working environment.
| Chemical Composition(wt%) | ||||||||
Ni | Cr | Mo | Co | Fe | W | Ti | C | O | |
HM-Hastelloy X | Bal. | 20.5-23 | 8-10 | 0.5-2.5 | 17-20 | 0.2-1 | <0.5 | 0.05-0.15 | ≤0.03 |
Apparent Density | ≥4.40 g/cm3 | Hall Flow Rate | ≤20 s/50g | ||||||
Particle Size | 15-45μm, 15-53μm, 45-106μm, 75-150μm, or customized | ||||||||

Hastelloy X Spherical Superalloy Powder should be stored in a sealed container in a dry and cool place, and should not be exposed to air for an extended period of time. We offer vacuum-sealed packaging including 100g/bag, 500g/bag, 1kg/bag, and 25kg/drum, or we can offer customized packaging as per specific requirements.

Heeger Materials respects your privacy, and we will NOT sell or provide your personal data to other third parties, or allow them to use your personal data for their own purposes. However, we would like to send you information from time to time by mail or email about our products and special offers in addition to the interest categories you've selected above. Read our Privacy Policy